All I needed to do was trowel the marine-tex into the delamination area and clamp with "C" clamps for 24 hours.
Still holding together. I'm not sure if the consistancy of the marine-tex would alow it to go through a large syringe or not. Maybe, if you let it heat up in the sun before mixing. It does get thinner the warmer it is.

Regards,
Mike