Phill,
If I recall correctly the 100 gm uni was less than half that of 200 gm woven carbon. So two layers of uni were the way for home builts if one wanted to use carbon.. Three around the case area (or kevlar).. Twin layers would be all one would need internally.. I dont recall what the cost was of kevlar prepreg...
When I did the maths years ago the cost of a prepreg carbon nomex wasnt that much more than the cost of a wet epoxy glass layup..

I suspect infusion is a little out of the home builders area.. But it looks good..

Saying this... The F16 highish weight doesnt require the use of these methods... But the infusion makes sense for commercial builders..

Stewart