Mixing ply and uni glass is not efficient. Ply has a stretch to failure of less than 1%. The uni is about 6%. So the ply has to fail completely before the glass is helping but about 17%. Better to use carbon with plywood in that case. Similar stretch to failure.
Something I had not thought about, but which explains my failed ply and glass foils