| Galvanic corrosion and the sacrificial anode #140297 04/17/08 11:25 AM 04/17/08 11:25 AM | Anonymous
Unregistered
| Anonymous
Unregistered | Does anyone use sacrificial anodes? If so, where do you attach them?
I sail exclusively in salt water and have seen some seriously corroded boats.. I would love to avoid this. I sail about 100 days a year on my 1 boat so I want to preserve it as much as I can.
I do rinse off my cat with some freshwater (all the blocks, cleats, travleres, and all areas where dissimilar metals are) every night if I leave the cat on the beach (Friday and sat nights), and bring it through the car/boat wash every Sunday when it leaves the beach.
Thanks, | | | Re: Galvanic corrosion and the sacrificial anode
[Re: ]
#140298 04/17/08 01:07 PM 04/17/08 01:07 PM |
Joined: Aug 2007 Posts: 342 Indianapolis, IN - Midwest USA... IndyWave
enthusiast
|
enthusiast
Joined: Aug 2007
Posts: 342 Indianapolis, IN - Midwest USA... | Man, the title of this thread would make a GREAT name for a band!
(Thanks to Dave Barry, who was always on the look-out for new band names!)
What - Me Worry?
2006 Hobie Wave 7358 "Ish Kabibble"
| | | Re: Galvanic corrosion and the sacrificial anode
[Re: IndyWave]
#140300 04/17/08 02:06 PM 04/17/08 02:06 PM | Anonymous
Unregistered
| Anonymous
Unregistered | I thought it sounded like a great book, or discovery channel show.... hehe but didnt want to get to long winded (first time for everything?) in my original post. | | | Re: Galvanic corrosion and the sacrificial anode
[Re: Jake]
#140301 04/17/08 02:07 PM 04/17/08 02:07 PM | Anonymous
Unregistered
| Anonymous
Unregistered | | | | Re: Galvanic corrosion and the sacrificial anode
[Re: ]
#140302 04/17/08 04:57 PM 04/17/08 04:57 PM |
Joined: Jul 2001 Posts: 1,200 Vancouver, BC Tornado
veteran
|
veteran
Joined: Jul 2001
Posts: 1,200 Vancouver, BC | Here's a question I've yet to find a suitable answer for...do sacraficial anodes only do their thing while in the water? Does it need to be immersed to complete the circuit and corrode the anode? Been thinking of adding one to my launch trailer...but if it only works when immersed, there's not much point.
Mike Dobbs Tornado CAN 99 "Full Tilt"
| | | Re: Galvanic corrosion and the sacrificial anode
[Re: ncik]
#140304 04/17/08 07:57 PM 04/17/08 07:57 PM |
Joined: Jul 2001 Posts: 1,200 Vancouver, BC Tornado
veteran
|
veteran
Joined: Jul 2001
Posts: 1,200 Vancouver, BC | Kewl...no anodes for my trailer! Only works when the circuit is closed, ie. when disimilar metals are immersed in a conducting solution. A dry boat will never corrode galvanically.
A good fresh water wash then left to dry is all that is required to reduce corrosion considerably.
Mike Dobbs Tornado CAN 99 "Full Tilt"
| | |
|