Does anyone use sacrificial anodes? If so, where do you attach them?

I sail exclusively in salt water and have seen some seriously corroded boats.. I would love to avoid this. I sail about 100 days a year on my 1 boat so I want to preserve it as much as I can.

I do rinse off my cat with some freshwater (all the blocks, cleats, travleres, and all areas where dissimilar metals are) every night if I leave the cat on the beach (Friday and sat nights), and bring it through the car/boat wash every Sunday when it leaves the beach.

Thanks,

-- Have You Seen This? --
Re: Galvanic corrosion and the sacrificial anode [Re: ] #140298
04/17/08 01:07 PM
04/17/08 01:07 PM
Joined: Aug 2007
Posts: 342
Indianapolis, IN - Midwest USA...
IndyWave Offline
enthusiast
IndyWave  Offline
enthusiast

Joined: Aug 2007
Posts: 342
Indianapolis, IN - Midwest USA...
Man, the title of this thread would make a GREAT name for a band!

(Thanks to Dave Barry, who was always on the look-out for new band names!)


What - Me Worry?


2006 Hobie Wave 7358
"Ish Kabibble"
Re: Galvanic corrosion and the sacrificial anode [Re: ] #140299
04/17/08 01:33 PM
04/17/08 01:33 PM
Joined: Jun 2001
Posts: 12,310
South Carolina
Jake Offline
Carpal Tunnel
Jake  Offline
Carpal Tunnel

Joined: Jun 2001
Posts: 12,310
South Carolina


Jake Kohl
Re: Galvanic corrosion and the sacrificial anode [Re: IndyWave] #140300
04/17/08 02:06 PM
04/17/08 02:06 PM

A
Anonymous
Unregistered
Anonymous
Unregistered
A



I thought it sounded like a great book, or discovery channel show.... hehe but didnt want to get to long winded (first time for everything?) in my original post.

Re: Galvanic corrosion and the sacrificial anode [Re: Jake] #140301
04/17/08 02:07 PM
04/17/08 02:07 PM

A
Anonymous
Unregistered
Anonymous
Unregistered
A



Great link, thanks...

Re: Galvanic corrosion and the sacrificial anode [Re: ] #140302
04/17/08 04:57 PM
04/17/08 04:57 PM
Joined: Jul 2001
Posts: 1,200
Vancouver, BC
Tornado Offline
veteran
Tornado  Offline
veteran

Joined: Jul 2001
Posts: 1,200
Vancouver, BC
Here's a question I've yet to find a suitable answer for...do sacraficial anodes only do their thing while in the water? Does it need to be immersed to complete the circuit and corrode the anode? Been thinking of adding one to my launch trailer...but if it only works when immersed, there's not much point.


Mike Dobbs
Tornado CAN 99 "Full Tilt"
Re: Galvanic corrosion and the sacrificial anode [Re: Tornado] #140303
04/17/08 06:07 PM
04/17/08 06:07 PM
Joined: Oct 2005
Posts: 951
Brisbane, Queensland, Australi...
ncik Offline
old hand
ncik  Offline
old hand

Joined: Oct 2005
Posts: 951
Brisbane, Queensland, Australi...
Only works when the circuit is closed, ie. when disimilar metals are immersed in a conducting solution. A dry boat will never corrode galvanically.

A good fresh water wash then left to dry is all that is required to reduce corrosion considerably.

Re: Galvanic corrosion and the sacrificial anode [Re: ncik] #140304
04/17/08 07:57 PM
04/17/08 07:57 PM
Joined: Jul 2001
Posts: 1,200
Vancouver, BC
Tornado Offline
veteran
Tornado  Offline
veteran

Joined: Jul 2001
Posts: 1,200
Vancouver, BC
Kewl...no anodes for my trailer!


Quote
Only works when the circuit is closed, ie. when disimilar metals are immersed in a conducting solution. A dry boat will never corrode galvanically.

A good fresh water wash then left to dry is all that is required to reduce corrosion considerably.


Mike Dobbs
Tornado CAN 99 "Full Tilt"
Re: Galvanic corrosion and the sacrificial anode [Re: ] #140305
04/21/08 11:17 PM
04/21/08 11:17 PM
Joined: Nov 2003
Posts: 130
CA
Glenn_Brown Offline
member
Glenn_Brown  Offline
member

Joined: Nov 2003
Posts: 130
CA
I use Duralac, attached between the dissimilar metals. (It's a paste. Barium Chromate, I think.)

--Glenn


Moderated by  Damon Linkous 

Search

Who's Online Now
0 registered members (), 2,533 guests, and 195 spiders.
Key: Admin, Global Mod, Mod
Newest Members
Darryl, zorro, CraigJ, PaulEddo2, AUS180
8150 Registered Users
Top Posters(30 Days)
Forum Statistics
Forums35
Topics22,989
Posts268,931
Members8,150
Most Online23,979
Sep 24th, 2025
--Advertisement--
Powered by UBB.threads™ PHP Forum Software 7.7.1