Originally Posted by Matt_Stone
The orange peel affect, is caused by applying too thick off the gun, to get auto finish thinner coats and more of it, what I saw in the pics is called fish eyed, means contamination on the cloths or on the work, usally siliconis the main cause and oil. other reasons undercoat not cured properly. Orange peel affect is on almost everything that is industral, as its a good strong coat and will last for years, auto finish is good bht need to be upkept


The paint rep dropped by today, showed him the pics of the boat and he also had a look at the effected steel work....

verdict => too heavy with the 2nd coat and way too hot when applied, the really bad areas are a contamination .

this is part of the effected steel work that was sprayed on the same day, oddly enough only half the beam was effected, the rest as we've since noted was in the shade and completely unaffected.

[Linked Image]